Carbon Steel SS 440
Material Group | |
---|---|
Material Group | Carbon Steel |
Alloy | SS 440 |
Equivalent Grades | |
Technology | CNC Machining & Turning / MIM Injections |
Mechanical Properties | |
---|---|
Elongation % | 4 |
Tensile Strength MPa | 1750 |
Yield Strength MPa | 1280 |
Shear Strength MPa | |
Hardness Brinell | 604 |
Physical Properties | |
---|---|
Density g/cm3 | 7.8 |
Melting Point (±50) °C | |
Thermal Conductivity W/mK | |
Coefficient of Thermal expension | 10.2 |
Electrical Conductivity %IACS |
Composition | |
---|---|
Al | |
Cu | |
Mg | |
Fe (max) | 78.4-83.4 |
Tin (max) | |
Ni (max) | |
Cr | 16-18 |
C | 0.60-0.75 |
Mo | 0.75 |
Mn | 1 |
Si | 1 |
Zn | |
Sn | |
Ca | |
Ni | |
Bi | |
Ti | |
S | 0.03 |
Sb | |
P | 0.04 |
Pb | |
Cd | |
Other |