Tool Steel H13 Annealed
Material Group | |
---|---|
Material Group | Tool Steel |
Alloy | H13 Annealed |
Equivalent Grades | SKD61 |
Technology | CNC Machining & Turning |
Mechanical Properties | |
---|---|
Elongation % | 21 |
Tensile Strength MPa | 690 |
Yield Strength MPa | 330 |
Shear Strength MPa | 430 |
Hardness Brinell | 210 |
Physical Properties | |
---|---|
Density g/cm3 | 7.8 |
Melting Point (±50) °C | 1420 |
Thermal Conductivity W/mK | 29 |
Coefficient of Thermal expension | |
Electrical Conductivity %IACS | 8.3 |
Composition | |
---|---|
Al | |
Cu | 0.25 |
Mg | |
Fe (max) | 88.8-92 |
Tin (max) | |
Ni (max) | 0.3 |
Cr | 4.8-5.5 |
C | 0.32-0.45 |
Mo | 1.1-1.8 |
Mn | 0.2-0.5 |
Si | 0.8-1.2 |
Zn | |
Sn | |
Ca | |
Ni | |
Bi | |
Ti | |
S | 0.03 |
Sb | |
P | 0.03 |
Pb | |
Cd | |
Other |