Aluminum B390
Material Group | |
|---|---|
| Material Group | Aluminum |
| Alloy | B390 |
| Equivalent Grades | ADC14 |
| Technology | Aluminum Casting |
Mechanical Properties | |
|---|---|
| Elongation % | 1 |
| Tensile Strength MPa | 317 |
| Yield Strength MPa | 250 |
| Shear Strength MPa | |
| Hardness Brinell | 120 |
Physical Properties | |
|---|---|
| Density g/cm3 | 2.71 |
| Melting Point (±50) °C | 580 |
| Thermal Conductivity W/mK | 134 |
| Coefficient of Thermal expension | 18 |
| Electrical Conductivity %IACS | 27 |
Composition | |
|---|---|
| Al | Remainder |
| Cu | 4.0-5.0 |
| Mg | 0.45-0.65 |
| Fe (max) | 1.3 |
| Tin (max) | |
| Ni (max) | 0.1 |
| Cr | |
| C | |
| Mo | |
| Mn | 0.5 |
| Si | 16.0-18.0 |
| Zn | 1.5 |
| Sn | |
| Ca | |
| Ni | |
| Bi | |
| Ti | |
| S | |
| Sb | |
| P | |
| Pb | |
| Cd | |
| Other | 0.2 |